激光增材制造高温合金材料与工艺研究进展 |
| 孙晓峰, 宋巍, 梁静静, 李金国, 周亦胄 |
|
Research and Development in Materials and Processes of Superalloy Fabricated by Laser Additive Manufacturing |
| SUN Xiaofeng, SONG Wei, LIANG Jingjing, LI Jinguo, ZHOU Yizhou |
| 图6 增材制造高温合金典型的微观组织及演变[ (a) columnar dendrite[ (b) characteristics of the molten pool[ (c) schematic diagram of equiaxed crystal growth[ (d) schematic diagram of structure evolution (G—temperature gradient)[ |
| Fig.6 Typical structure and evolution of additive manufacturing superalloys |
|