激光增材制造高温合金材料与工艺研究进展 |
| 孙晓峰, 宋巍, 梁静静, 李金国, 周亦胄 |
|
Research and Development in Materials and Processes of Superalloy Fabricated by Laser Additive Manufacturing |
| SUN Xiaofeng, SONG Wei, LIANG Jingjing, LI Jinguo, ZHOU Yizhou |
| 图5 激光增材制造技术修复的高温合金单晶叶片[ (a) repaired blade (b) EBSD mapping |
| Fig.5 Superalloy single-crystal parts fabricated by laser additive manufacturing[ |
|