高强韧钛合金组成相成分和形态的精细调控 |
| 杨锐, 马英杰, 雷家峰, 胡青苗, 黄森森 |
|
Toughening High Strength Titanium Alloys Through Fine Tuning Phase Composition and Refining Microstructure |
| YANG Rui, MA Yingjie, LEI Jiafeng, HU Qingmiao, HUANG Sensen |
| 图5 多种二元钛合金中ω-β相能量差随成分x的变化[ |
| Fig.5 Energy difference (ΔEω-β) between ω and β phases of binary Ti-xM (M = Zr, V, Nb, Mo, Cr) alloys vs content of M (x)[ |
|