高强韧钛合金组成相成分和形态的精细调控 |
| 杨锐, 马英杰, 雷家峰, 胡青苗, 黄森森 |
|
Toughening High Strength Titanium Alloys Through Fine Tuning Phase Composition and Refining Microstructure |
| YANG Rui, MA Yingjie, LEI Jiafeng, HU Qingmiao, HUANG Sensen |
| 图4 Ti-3Al-5Mo-4.5V合金不同热处理条件下的真应力-真应变曲线及加工硬化率曲线 |
| Fig.4 True strain-stress curves (a) and work hardening rate curves (b) of Ti-3Al-5Mo-4.5V specimens under different heat-treatment conditions (750 representing 750oC, 2 h, water quenching; 750 + 300 representing 750oC, 2 h, water quenching + 300oC, 6 h, air cooling; 750 + 500 representing 750oC, 2 h, water quenching + 500oC, 6 h, air cooling) |
|