高强亚稳β钛合金变形机制及其组织调控方法 |
| 李金山, 唐斌, 樊江昆, 王川云, 花珂, 张梦琪, 戴锦华, 寇宏超 |
|
Deformation Mechanism and Microstructure Control of High Strength Metastable β Titanium Alloy |
| LI Jinshan, TANG Bin, FAN Jiangkun, WANG Chuanyun, HUA Ke, ZHANG Mengqi, DAI Jinhua, KOU Hongchao |
| 图11 热力耦合作用下Ti-5553合金DRV/DRX和相变过程竞争机制及相转变曲线(TTT)示意图[ |
| Fig.11 Schematics of the competition between dynamic recovery/dynamic recrystallization (DRV/DRX) and phase transformation (The two insets are schematic diagrams of phase transformation and DRV/DRX, respectively. Ttrans—transition temperature) (a), and time-temperature-transformation (TTT) curves of Ti-5553 alloy under thermo-mechanical conditions (b)[ |
|