高强亚稳β钛合金变形机制及其组织调控方法 |
| 李金山, 唐斌, 樊江昆, 王川云, 花珂, 张梦琪, 戴锦华, 寇宏超 |
|
Deformation Mechanism and Microstructure Control of High Strength Metastable β Titanium Alloy |
| LI Jinshan, TANG Bin, FAN Jiangkun, WANG Chuanyun, HUA Ke, ZHANG Mengqi, DAI Jinhua, KOU Hongchao |
| 图10 热机械过程的不同阶段和对应微观组织演变及其示意图[ |
| Fig.10 Different stages of the thermomechanical process (T—temperature) (a) and the associated microstructural evolutions with their geometrical simplifications (b) [ |
|