镁基储氢合金动力学调控及电化学性能 |
| 朱敏, 欧阳柳章 |
|
Kinetics Tuning and Electrochemical Performance of Mg-Based Hydrogen Storage Alloys |
| ZHU Min, OUYANG Liuzhang |
| 图7 球磨60 h制备的Mg0.50Ni0.50、Mg0.45Ti0.05Ni0.50和Mg0.40Ti0.10Ni0.50合金电极经30 cyc循环后的TG曲线和DSC曲线[ |
| Fig.7 TG (a) and DSC (b) results of the 60 h milled Mg0.50Ni0.50, Mg0.45Ti0.05Ni0.50, and Mg0.40Ti0.10Ni0.50 alloy electrodes at discharge state after 30 cyc[ |
|