多晶Ni-Mn-X相变合金的织构化与功能行为 |
| 左良, 李宗宾, 闫海乐, 杨波, 赵骧 |
|
Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys |
| ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang |
| 图17 Ni46Co3Mn35Cu2In14合金2次测量获得的ΔSM及ΔTad随温度变化[ |
| Fig.17 Temperature dependence of ΔSM under the magnetic field change of 5 T (a) and ΔTad under the magnetic field change of 1.5 T (b) for the first and second cycles of measurement for the Ni46Co3Mn35Cu2In14 alloy (ΔSM—isothermal magnetic entropy change)[ |
|