多晶Ni-Mn-X相变合金的织构化与功能行为 |
| 左良, 李宗宾, 闫海乐, 杨波, 赵骧 |
|
Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys |
| ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang |
| 图16 定向凝固Ni45.3Co5.1Mn36.1In13.5合金的M(T)曲线及1.5 T磁场下的ΔTad随温度变化[ |
| Fig.16 Temperature dependence of magnetization M(T) curves under various magnetic fields (a) and ΔTad values under the field change of 1.5 T (b) for the directionally solidified Ni45.3Co5.1Mn36.1In13.5 alloy (ΔTad—adiabatic temperature variation)[ |
|