多晶Ni-Mn-X相变合金的织构化与功能行为
左良, 李宗宾, 闫海乐, 杨波, 赵骧

Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys
ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang
图15 机械训练后定向凝固Ni50Mn28.5Ga21.5合金样品的磁感生应变曲线[80]
Fig.15 Magnetic field-induced strain as a function of applied field (a) and its reversible behavior (b) for the directionally solidified Ni50Mn28.5Ga21.5 alloy after mechanical training (μ0H—magnetic field)[80]