多晶Ni-Mn-X相变合金的织构化与功能行为 |
| 左良, 李宗宾, 闫海乐, 杨波, 赵骧 |
|
Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys |
| ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang |
| 图6 奥氏体与7M马氏体之间惯习面的TEM高分辨像(电子束沿<1 1 1>A晶带轴)[ |
| Fig.6 A high-resolution TEM image of the austenite-7M martensite interface viewed along <1 1 1>A[ |
|