纳米孪晶金属和纳米孪晶共价材料的力学行为
温斌, 田永君

Mechanical Behaviors of Nanotwinned Metals and Nanotwinned Covalent Materials
WEN Bin, TIAN Yongjun
图11 纳米孪晶金刚石硬度的计算值与实验值对比[51]
(a) population of yielded grains as a function of uniaxial stress, based on the Sachs model, which is illustrated schematically in the inset (When the proportion of yielded grains reaches 90%, the corresponding uniaxial stress is defined as the yield stress. The curve is an example for an nt-diamond sample with twin thickness of 5 nm and grain size of 20 nm)
(b) calculated hardness of nt-diamond as a function of twin thickness compared to experimental ones (The inset shows the proportion of yielded grain by different slip modes at grain size of 20 nm)
Fig.11 Calculated hardness compared to experimental data for nt-diamond as a function of twin thickness [51]