纳米孪晶金属和纳米孪晶共价材料的力学行为
温斌, 田永君

Mechanical Behaviors of Nanotwinned Metals and Nanotwinned Covalent Materials
WEN Bin, TIAN Yongjun
图9 纳米孪晶金刚石的微结构和位错滑移模式示意图[51]
(a) a polycrystalline nt-diamond microstructure consists of subparallel nanoscale twin lamella embedded in submicrometer-sized grains (Grains have random orientations)
(b) three dislocation slip modes in nt-diamond: slip transfer (slip mode I), confined layer slip (slip mode II), and paralleled to TB slip mode (slip mode III) (Tetrahedrons ABCD and ATBTCTDT represent the Burgers vectors of dislocations in the parent crystal and its twined counterpart, respectively. The partial dislocations are denoted by Roman-Greek pairs (such as Aδ, Cδ, Bδ, etc.))
Fig.9 Schematics of the nt-diamond microstructure and slip modes[51]