镁合金塑性加工技术发展及应用
潘复生, 蒋斌

Development and Application of Plastic Processing Technologies of Magnesium Alloys
PAN Fusheng, JIANG Bin
图4 AZ31镁合金宽幅板材(1.5~2.2 m宽)
Fig.4 Wide sheet of AZ31 magnesium alloy (The width is 1.5-2.2 m)