机器学习在材料研发中的应用 |
| 谢建新, 宿彦京, 薛德祯, 姜雪, 付华栋, 黄海友 |
|
Machine Learning for Materials Research and Development |
| XIE Jianxin, SU Yanjing, XUE Dezhen, JIANG Xue, FU Huadong, HUANG Haiyou |
| 图1 材料高通量实验结合机器学习预测镍基高温合金的有害相[ |
| Fig.1 Schematic workflow of phase prediction via high-throughput experiments and machine learning of Ni-base superalloys[ |
|