渐进法向力对金属材料微米划痕响应的影响 |
| 刘明, 严富文, 高诚辉 |
|
Effects of Progressive Normal Force on Microscratch Responses of Metallic Materials |
| LIU Ming, YAN Fuwen, GAO Chenghui |
| 图7 稳定弹性恢复率、屈服强度和努氏硬度与稳定划痕硬度的关系 |
| Fig.7 Relationships among Rea, yield strength (σy), Knoop hardness (Hk), and Have |
|