含有化合物相的共晶转变理论模型 |
| 许军锋, 张宝东, Peter K Galenko |
|
Model of Eutectic Transformation Involving Intermetallic Compound |
| XU Junfeng, ZHANG Baodong, Peter K Galenko |
| 图5 实验与计算结果对比 (a) ΔT-V curves of Al-Al2Cu alloy (ΔT—undercooling) (b) V-λ curves of Al-Al2Cu alloy and experimental data[ (c) interfacial concentration distribution C(x, z) of Al-Al2Cu alloy at two growth rates (d) calculation results and experiments[ |
| Fig.5 Results of the experiments and calculation of alloys |
|