含有化合物相的共晶转变理论模型
许军锋, 张宝东, Peter K Galenko

Model of Eutectic Transformation Involving Intermetallic Compound
XU Junfeng, ZHANG Baodong, Peter K Galenko
图4 Al-Al2Cu合金相图[30]和CuZr-CuZr2合金相图[31]
Fig.4 Phase diagrams of Al-Al2Cu alloy[30] (a) and CuZr-CuZr2 alloy[31] (b) (T—temperature)