Al19.3Co15Cr15Ni50.7高熵合金的热变形行为 |
| 刘庆琦, 卢晔, 张翼飞, 范笑锋, 李瑞, 刘兴硕, 佟雪, 于鹏飞, 李工 |
|
Thermal Deformation Behavior of Al19.3Co15Cr15Ni50.7 High Entropy Alloy |
| LIU Qingqi, LU Ye, ZHANG Yifei, FAN Xiaofeng, LI Rui, LIU Xingshuo, TONG Xue, YU Pengfei, LI Gong |
| 图13 不同应变条件下的热加工图 (a) ε = 0.3 (b) ε = 0.4 (c) ε = 0.5 (d) ε = 0.6 (e) ε = 0.7 |
| Fig.13 Heat working diagrams under different variable conditions (The numbers in the figures are the values of dissipation rate, the shadows represent instable zones) |
|