Al19.3Co15Cr15Ni50.7高熵合金的热变形行为 |
| 刘庆琦, 卢晔, 张翼飞, 范笑锋, 李瑞, 刘兴硕, 佟雪, 于鹏飞, 李工 |
|
Thermal Deformation Behavior of Al19.3Co15Cr15Ni50.7 High Entropy Alloy |
| LIU Qingqi, LU Ye, ZHANG Yifei, FAN Xiaofeng, LI Rui, LIU Xingshuo, TONG Xue, YU Pengfei, LI Gong |
| 图9 α、n、lnA、Q与应变的关系曲线 |
| Fig.9 The curves of α (a), n (b), lnA (c), and Q (d) with strain |
|