FeCrNiMo激光熔覆层组织与摩擦磨损行为 |
| 赵万新, 周正, 黄杰, 杨延格, 杜开平, 贺定勇 |
|
Microstructure and Frictional Wear Behavior of FeCrNiMo Alloy Layer Fabricated by Laser Cladding |
| ZHAO Wanxin, ZHOU Zheng, HUANG Jie, YANG Yange, DU Kaiping, HE Dingyong |
| 图11 熔覆层在不同温度下表面磨痕形貌 |
| Fig.11 Worn morphologies of the cladding layer under 25oC (a), 300oC (b), and 600oC (c) conditions |
|