FeCrNiMo激光熔覆层组织与摩擦磨损行为 |
| 赵万新, 周正, 黄杰, 杨延格, 杜开平, 贺定勇 |
|
Microstructure and Frictional Wear Behavior of FeCrNiMo Alloy Layer Fabricated by Laser Cladding |
| ZHAO Wanxin, ZHOU Zheng, HUANG Jie, YANG Yange, DU Kaiping, HE Dingyong |
| 图2 熔覆层沿厚度方向的微观组织 |
| Fig.2 Microstructures of the cladding layer along the thickness direction, in terms of integral cross-section (a), top section (b), middle section (c), and bottom section (d) (H—thickness, DR—dendritic region, IDR—inter-dendritic region) |
|