齿轮钢铸态点状偏析及其在热轧棒材中的演变 |
| 张壮, 李海洋, 周蕾, 刘华松, 唐海燕, 张家泉 |
|
As-Cast Spot Segregation of Gear Steel and Its Evolution in the Rolled Products |
| ZHANG Zhuang, LI Haiyang, ZHOU Lei, LIU Huasong, TANG Haiyan, ZHANG Jiaquan |
| 图10 铸坯点状偏析至棒材带状缺陷的形貌演变示意图 |
| Fig.10 Schematics of morphological evolution of the complex spot segregation through rolling |
|