45CrNiMoVA钢脉冲磁处理的强化机理 |
|||||||||||||||
| 栾晓圣, 梁志强, 赵文祥, 石贵红, 李宏伟, 刘心藜, 祝国荣, 王西彬 | |||||||||||||||
|
Strengthening Mechanism of 45CrNiMoVA Steel by Pulse Magnetic Treatment |
|||||||||||||||
| LUAN Xiaosheng, LIANG Zhiqiang, ZHAO Wenxiang, SHI Guihong, LI Hongwei, LIU Xinli, ZHU Guorong, WANG Xibin | |||||||||||||||
| 表1 45CrNiMoVA钢脉冲磁化处理实验方案 |
|||||||||||||||
| Table 1 Experimental scheme of pulse magnetization treatment for 45CrNiMoVA steel |
|||||||||||||||
|
|||||||||||||||