45CrNiMoVA钢脉冲磁处理的强化机理 |
| 栾晓圣, 梁志强, 赵文祥, 石贵红, 李宏伟, 刘心藜, 祝国荣, 王西彬 |
|
Strengthening Mechanism of 45CrNiMoVA Steel by Pulse Magnetic Treatment |
| LUAN Xiaosheng, LIANG Zhiqiang, ZHAO Wenxiang, SHI Guihong, LI Hongwei, LIU Xinli, ZHU Guorong, WANG Xibin |
| 图6 磁化处理前后45CrNiMoVA钢表面残余应力的变化 |
| Fig.6 The surface residual stress changes of magnetized and unmagnetized 45CrNiMoVA steels |
|