AZ31镁合金表面苯丙氨酸、甲硫氨酸和天冬酰胺诱导Ca-P涂层耐蚀性能比较 |
| 王雪梅, 殷正正, 于晓彤, 邹玉红, 曾荣昌 |
|
Comparison of Corrosion Resistance of Phenylalanine, Methionine, and Asparagine-Induced Ca-P Coatings on AZ31 Magnesium Alloys |
| WANG Xuemei, YIN Zhengzheng, YU Xiaotong, ZOU Yuhong, ZENG Rongchang |
| 图11 AZ31镁合金、Ca-P涂层和3种氨基酸诱导Ca-P涂层浸泡160 h后的宏观形貌和SEM像 |
| Fig.11 Digital camera photographs (a, d, g, j, m) and SEM images (b, c, e, f, h, i, k, l, n, o) after 160 h immersion for AZ31 Mg alloy (a-c), Ca-P coating (d-f), Ca-PPhe coating (g-i), Ca-PMet coating (j-l), and Ca-PAsn coating (m-o) |
|