AZ31镁合金表面苯丙氨酸、甲硫氨酸和天冬酰胺诱导Ca-P涂层耐蚀性能比较 |
| 王雪梅, 殷正正, 于晓彤, 邹玉红, 曾荣昌 |
|
Comparison of Corrosion Resistance of Phenylalanine, Methionine, and Asparagine-Induced Ca-P Coatings on AZ31 Magnesium Alloys |
| WANG Xuemei, YIN Zhengzheng, YU Xiaotong, ZOU Yuhong, ZENG Rongchang |
| 图 7 AZ31镁合金及其Ca-P涂层和3种氨基酸诱导Ca-P涂层的极化曲线 |
| Fig.7 Polarization curves of AZ31Mg alloy, Ca-P coating, Ca-PPhe coating, Ca-PMet coating, and Ca-PAsn coating (Eb—broken shield potential) |
|