AZ31镁合金表面苯丙氨酸、甲硫氨酸和天冬酰胺诱导Ca-P涂层耐蚀性能比较 |
| 王雪梅, 殷正正, 于晓彤, 邹玉红, 曾荣昌 |
|
Comparison of Corrosion Resistance of Phenylalanine, Methionine, and Asparagine-Induced Ca-P Coatings on AZ31 Magnesium Alloys |
| WANG Xuemei, YIN Zhengzheng, YU Xiaotong, ZOU Yuhong, ZENG Rongchang |
| 图4 3种氨基酸诱导Ca-P涂层的XPS谱宽谱和精细谱 (b, e, h) C1s (c, f, i) N1s |
| Fig.4 XPS survey plots (a, d, g) and high-resolution spectra (b, c, e, f, h, i) of Ca-PPhe coating (a-c), Ca-PMet coating (d-f), and Ca-PAsn coating (g-i) |
|