AZ31镁合金表面苯丙氨酸、甲硫氨酸和天冬酰胺诱导Ca-P涂层耐蚀性能比较 |
| 王雪梅, 殷正正, 于晓彤, 邹玉红, 曾荣昌 |
|
Comparison of Corrosion Resistance of Phenylalanine, Methionine, and Asparagine-Induced Ca-P Coatings on AZ31 Magnesium Alloys |
| WANG Xuemei, YIN Zhengzheng, YU Xiaotong, ZOU Yuhong, ZENG Rongchang |
| 图 3 AZ31镁合金表面Ca-P 涂层和3种氨基酸诱导Ca-P涂层截面形貌的SEM像和元素分布 |
| Fig.3 Cross-sectional SEM images and corresponding Ca and P mapping images of Ca-P coating (a), Ca-PPhe coating (b), Ca-PMet coating (c), and Ca-PAsn coating (d) on AZ31 magnesium alloy surface |
|