锻造-增材复合制造Ti-6Al-4V合金结合区显微组织及力学性能 |
| 马健凯, 李俊杰, 王志军, 王俞鉴, 王锦程 |
|
Bonding Zone Microstructure and Mechanical Properties of Forging-Additive Hybrid Manufactured Ti-6Al-4V Alloy |
| MA Jiankai, LI Junjie, WANG Zhijun, WANG Yujian, WANG Jincheng |
| 图10 不同线能量密度下锻造-增材复合制造Ti-6Al-4V合金结合区试样的应力-应变曲线 |
| Fig.10 Stress-strain curves of the bonding zone samples in forging-additive hybrid manufactured Ti-6Al-4V alloy under different linear energy densities |
|