锻造-增材复合制造Ti-6Al-4V合金结合区显微组织及力学性能 |
| 马健凯, 李俊杰, 王志军, 王俞鉴, 王锦程 |
|
Bonding Zone Microstructure and Mechanical Properties of Forging-Additive Hybrid Manufactured Ti-6Al-4V Alloy |
| MA Jiankai, LI Junjie, WANG Zhijun, WANG Yujian, WANG Jincheng |
| 图3 不同线能量密度下锻造-增材复合制造Ti-6Al-4V合金增材区的微观组织及其特征尺寸 |
| Fig.3 Microstructures (a-c) and feature sizes (d-f) of α phase of the laser deposition zone in forging-additive hybrid manufactured Ti-6Al-4V alloy under linear energy densities of 100 J/mm (a, d), 133 J/mm (b, e), and 200 J/mm (c, f) (Insets in Figs.3a-c show the enlarged views. α: dark area, β: bright bar, αGB—grain boundary α phase) |
|