连铸中间包加热技术及其冶金功能研究进展 |
| 唐海燕, 刘锦文, 王凯民, 肖红, 李爱武, 张家泉 |
|
Progress and Perspective of Functioned Continuous Casting Tundish Through Heating and Temperature Control |
| TANG Haiyan, LIU Jinwen, WANG Kaimin, XIAO Hong, LI Aiwu, ZHANG Jiaquan |
| 图1 中间包等离子加热装置示意图[ |
| Fig.1 Schematic of plasma heating device[ |
|