高温时效处理对S31042耐热钢组织和蠕变性能的影响
郭倩颖1, 李彦默2, 陈斌2, 丁然1, 余黎明1, 刘永长1()
Effect of High-Temperature Ageing on Microstructure and Creep Properties of S31042 Heat-Resistant Steel
GUO Qianying1, LI Yanmo2, CHEN Bin2, DING Ran1, YU Liming1, LIU Yongchang1()

图2. 固溶态和时效态S31042钢样品中析出相的TEM像及EDS

Fig.2. TEM images (a, c) and EDS (b, d) of the precipitates in solution-treated (a, b) and ageing-treated (c, d) S31042 steel samples