高能球磨结合粉末冶金法制备碳纳米管增强7055Al复合材料的微观组织和力学性能
毕胜1,2, 李泽琛3, 孙海霞3, 宋保永3, 刘振宇1(), 肖伯律1, 马宗义1
Microstructure and Mechanical Properties of Carbon Nanotubes-Reinforced 7055Al Composites Fabricated by High-Energy Ball Milling and Powder Metallurgy Processing
BI Sheng1,2, LI Zechen3, SUN Haixia3, SONG Baoyong3, LIU Zhenyu1(), XIAO Bolv1, MA Zongyi1

图8. 不同体系的CNT/Al复合材料的力学性能

Fig.8. Mechanical properties of CNT/Al composites with different matrices