基于热力学和动力学协同的析出相模拟
|
|
Precipitation Modeling via the Synergy of Thermodynamics and Kinetics
|
|
图10. Al-2%Cu (原子分数)合金中θ'在473 K析出的尺寸演化和析出序列GP区→θ"→θ' [ |
Fig.10. The size evolution of θ' at 473 K (a) and the precipitation sequence, i.e. GP zone→θ"→θ' (b) in Al-2%Cu (atomic fraction) alloy (The abbreviations FP, MD, FPE, and PFM represent first-principles, molecular dynamics, Fokker-Planck equation, and phase field method, respectively)[ |
![]() |