基于热力学和动力学协同的析出相模拟
|
|
Precipitation Modeling via the Synergy of Thermodynamics and Kinetics
|
|
图7. 不同空间尺度计算模块间关联的多尺度模型图解[ |
Fig.7. Schematic of the multiscale model, showing different constituent models and their links along with their associated length scales (Fvibrational—free energy contributed from lattice vibration, Fconfigurational—configurational free energy)[ |
![]() |