难熔高熵合金在反应堆结构材料领域的机遇与挑战
|
|
Opportunity and Challenge of Refractory High-Entropy Alloys in the Field of Reactor Structural Materials
|
|
图7. AlMo0.5NbTa0.5TiZr合金的STEM-HAADF像及其快速Fourier变换,立方状无序bcc结构析出相被连续通道状有序B2基体相分割[ |
Fig.7. STEM-HAADF images and the fast Fourier transforms of AlMo0.5NbTa0.5TiZr showing cuboidal precipitates of a disordered bcc phase are separated by ordered B2 phase for the dark channels[ |
![]() |