难熔高熵合金在反应堆结构材料领域的机遇与挑战
李天昕1, 卢一平1,2(), 曹志强1, 王同敏1, 李廷举1
Opportunity and Challenge of Refractory High-Entropy Alloys in the Field of Reactor Structural Materials
LI Tianxin1, LU Yiping1,2(), CAO Zhiqiang1, WANG Tongmin1, LI Tingju1

图3. 单相(S)与多相(M)难熔高熵合金在1200℃的屈服强度(σ0.21200)与熔点(Tm)的关系[11]

Fig.3. Yield strength at 1200oC (σ0.21200) of single-phase (S) and multi-phase (M) refractory high-entropy alloys as a function of the melting temperature (Tm)[11]