形状记忆合金弹热制冷效应的研究现状
|
|
Research Progress in Elastocaloric Cooling Effect Basing on Shape Memory Alloy
|
|
图7. 几类代表性弹热制冷材料的等温熵变(ΔSiso)和绝热温度变化(ΔTadi)的对比 |
Fig.7. Comparisons of several typical shape memory alloy as elastocaloric materials including isothermal entropy change (ΔSiso) and adiabatic temperature change (ΔTadi) |
![]() |