形状记忆合金弹热制冷效应的研究现状
|
|
Research Progress in Elastocaloric Cooling Effect Basing on Shape Memory Alloy
|
|
图5. 根据文献[ |
Fig.5. The inverse elastocaloric effect in the Ti-Ni shape memory alloy exhibiting aligned Ti3Ni4 precipitatesdrew according to Ref.[ |
![]() |