形状记忆合金弹热制冷效应的研究现状
|
|
Research Progress in Elastocaloric Cooling Effect Basing on Shape Memory Alloy
|
|
图3. 快速拉伸与卸载过程中,红外探测所得Ti-Ni形状记忆合金样品温度的演变[ |
Fig.3. Temperature distributions (in oC, detected by infrared camera) of Ti-Ni shape memory alloy during the quick loading and unloading processes (Δε—strain amplitude)[ |
![]() |