形状记忆合金弹热制冷效应的研究现状
|
|
Research Progress in Elastocaloric Cooling Effect Basing on Shape Memory Alloy
|
|
图2. Ti-Ni形状记忆合金拉伸时弹热温度变化测试系统的示意图 |
Fig.2. Schematic showing of Ti-Ni shape memory alloy elastocaloric temperature change test during tension |
![]() |