镍基合金焊接裂纹研究现状
余磊, 曹睿
Welding Crack of Ni-Based Alloys: A Review
YU Lei, CAO Rui
表2
几种镍基合金产生组分液化的沉淀相
[
8
,
57
~
62
]
Table 2
Precipitate of component liquation in Ni-based alloys
[
8
,
57
-
62
]
Alloy
Precipitate
Ref.
Inconel 718
M
C
[
8
]
Inconel 738
γ'
,
M
C,
M
3
B
2
, Ni-Zr intermetallics
[
57
,
58
]
Inconel 617
M
23
(C, B)
6
[
59
]
Inconel 939
γ'
,
M
C
[
60
]
Rene 80
γ'
,
M
5
B
3
[
61
]
K465
γ'
,
M
C
[
62
]