用慢正电子束研究H/He中性束辐照W-ZrC合金中的缺陷演化
田雪芬1, 刘翔2, 龚敏1, 张培源1, 王康3, 邓爱红1()
Defect Evolution in H/He Neutral Beam Irradiated W-ZrC Alloy Using Positron Annihilation Spectroscopy
TIAN Xuefen1, LIU Xiang2, GONG Min1, ZHANG Peiyuan1, WANG Kang3, DENG Aihong1()

图1. SRIM模拟H/He中性束辐照W-ZrC后H和He含量、以及对应的损伤随深度分布

Fig.1. SRIM calculation results of H and He implantation profiles in W-ZrC (a), and the corresponding damage profiles (b)