放电等离子烧结TA15钛合金及石墨烯增强TA15复合材料微观组织与力学性能
林彰乾1,2, 郑伟3, 李浩1,2, 王东君1,2()
Microstructures and Mechanical Properties of TA15 Titanium Alloy and Graphene Reinforced TA15 Composites Prepared by Spark Plasma Sintering
LIN Zhangqian1,2, ZHENG Wei3, LI Hao1,2, WANG Dongjun1,2()

图5. 石墨烯增强TA15复合材料的XRD谱、Raman光谱、Raman面扫描、SEM像与压缩力学性能

Fig.5. XRD spectrum (a), Raman spectrum (b), Raman surface distribution (The inset shows the corresponding Raman mapping in the white rectangle) (c), SEM image (d), and compressive stress-strain curves (e) of graphene-reinforced TA15 composites