微合金化元素La对亚共晶Al-Si合金凝固组织与力学性能的影响
郑秋菊1,2, 叶中飞3, 江鸿翔1, 卢明3, 张丽丽1, 赵九洲1,2()
Effect of Micro-Alloying Element La on Solidification Microstructure and Mechanical Properties of Hypoeutectic Al-Si Alloys
ZHENG Qiuju1,2, YE Zhongfei3, JIANG Hongxiang1, LU Ming3, ZHANG Lili1, ZHAO Jiuzhou1,2()

图5. 含0.10%La的Al-6Si合金中稀土化合物和共晶Si的BEI像及EPMA元素面分布

Fig.5. Backscattered electron image (BEI) and EPMA mappings of the eutectic Si and La-rich phase particles in the Al-6Si alloy with 0.10%La addition