Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals
WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili
表3 金属粉末在生理盐水和含有蛋白质的溶液中浸泡16 h后,金属离子的释放量[29] (10-6)
Table 3 Analyses of metals in saline and protein solutions after 16 h exposure[29]
MetalSalineAlbuminFibrinogen
Aluminum1.301.481.00
Chromium0.502.380.70
Cobalt1.5031.5040.95
Copper3.7216996.60
Molybdenum514390355
Nickel4.807.709.50
Titanium0.20.20.2