[an error occurred while processing this directive]
蛋白质吸附对医用金属材料体外腐蚀行为的影响
王鲁宁1,2(), 刘丽君1, 岩雨1,3, 杨坤1, 陆黎立1
Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals
WANG Luning1,2(), LIU Lijun1, YAN Yu1,3, YANG Kun1, LU Lili1

图9. BSA吸附过程中,钛合金/液体界面之间电荷转移的理论模型[55]

Fig.9. Theoretical model of charged double layer showing the transfer of charge at the metal/oxide/protein interfaces before (a) and during (b) the corrosion process[55]