UO2烧结过程的相场模拟
孙正阳, 杨超, 柳文波

Phase Field Simulations of the Sintering Process of UO2
SUN Zhengyang, YANG Chao, LIU Wenbo
表1 UO2的物理参数[31,32,34]
Table 1 Physical parameters of UO2 at 2000 K[31,32,34]
Physical parameterValueRef.
Ds8.8258×10-11 m2·s-1[31]
Dgb7.8998×10-13 m2·s-1[32]
Dl7.8998×10-15 m2·s-1[34]
γs0.6 J·m-2[34]
γgb0.3 J·m-2[34]
δ6 nm[34]