[an error occurred while processing this directive]
UO2烧结过程的相场模拟
孙正阳1,2, 杨超3, 柳文波1,2()
Phase Field Simulations of the Sintering Process of UO2
SUN Zhengyang1,2, YANG Chao3, LIU Wenbo1,2()

图4. 不同形状晶粒的烧结颈的对数增长曲线

Fig.4. Logarithmic neck growth curves of two different shapes (l—neck length, t—time step)